SPVD CN
The SPVD CN is a kind of silver gray coating. It has great adherence power and good corrosion resistance and oxidation resistance. When the mechnical parts and moulds are PVD coated by SPVD CN, the wearing resistance and lubricity will be improved. Compared with the SPVD TN coating, the corrosion resistance ability of SPVD CN against water solution is more great. The higher surface hardness, lower coefficient of friction and lower residual stress of SPVD CN make it adapt to the occasions which need the above characters.

SPVD CNThe SPVD CN coating has very big hardness value:HV1700-2100, good corrosion resistance and oxidation resistance(700¡æ), great adherence power and can be coated at low temperature(200-400¡æ). It is very proper to be applied on the moulds, and better than traditional Cr plating in wear resistance. These good characters of SPVD CN will make it replace the Chemical plating of Cr which is a outdated technology in the surface treatment of moulds. It is often applied on the cutting tools used to cut brass products, shape forming moulds, and mechanical parts which need good wear resistance and corrosion resistance.
Performance Introduction£º


Material of coating
Appearance Hardness(HV) Coefficient of friction Internal stress Temperature of processing(¡æ) Temperature of oxidation resistance(¡æ) Thickness of coating(¦Ìm)
SPVD CN SPVD CN 1700∼2100 0.3 -1.5 400 700 1∼5
silver

The comparation of chemical plating Cr, SPVD CN and PVD TiN on moulds:

Coatings SPVD CN chemical plating Cr PVD TiN
Thickness£¨¦Ìm£© 2-10 20-50 2-10
Hardness(HV) 1700-2100 750-1000 2000-2400
Antioxidant temperature 800 ¡æ ----- 500 ¡æ
Acid crossion resistance excellent bad bad
Stripping ability excellent ordinary ordinary
Lifetime(take shape forming mould as an example) 350,000 times 100,000 times 180,000 times

The example of SPVD CN applied on moulds:
Applied moulds Hardness of material Thickness of SPVD CN (um) Processed material Thickness of processed material (mm) Roughness of the surface of the product(Ra) Temperature of the product(¡æ) Lifetime improved (times)
Aluminium alloy founded mould AISIH11/HRC52 5.5 silicon aluminum
alloy
forming by found 0.25 720 2
forming/
cutted mixed mould
DINX210CrN12/HRC60 4.5 corssion resistance
low carbon alloy stainless steel
panel
0.5 0.40 50 3.5
forming by cold processing/
deep pump mixed mould
AISID3/HRC60 5.5 low carbon alloy steel panel 1.0 0.40 50 6
automatically gradually going deep pump mixed mould AISID2/HRC62 4.0 DIN 1624 steel panel 0.2 0.06 120 5
mould forming by cold processing HSS/HRC62 4.0 stainless steel panel 1.5 0.10 50 4
mould forming by cold processing/
deep pump mixed
AISID3/HRC62 5.5 low carbon alloy steel panel 0.5 0.10 70 4.5